Nonlinear piezoresistive effect of 4H–SiC for applications of high temperature pressure sensors
|
|
Meng Meng, Renli Fu, Xuhai Liu
|
59 |
38 |
18105–18119 |
2024 |
0.0 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
The dissolution behavior of crystal-originated particle in 300 mm Czochralski silicon under argon annealing
|
|
Hao Wang, Yun Liu, Xing Wei
|
59 |
38 |
18120–18129 |
2024 |
6.82 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Cu–CeO2/YSZ electrodes for SOFCs: role of cermet meso/nanostructure in methane oxidation
|
|
Edgar M. Sánchez Faba, Horacio E. Troiani, Corina M. Chanquía
|
59 |
38 |
18130–18145 |
2024 |
4.84 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Exploring the evolution and damage behaviors of multidimensional defects surrounding film holes in single-crystal nickel-based superalloys
|
|
Xing Ai, Zheng Wang, Fenghua Luo
|
59 |
38 |
18146–18158 |
2024 |
0.0 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Thermodynamic re-modeling of the binary Al–Mo and ternary Al–Fe–Mo systems based on novel experimental data
|
|
I. Fartushna, V. Witusiewicz, M. Bulanova
|
59 |
38 |
18159–18195 |
2024 |
5.82 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Enhancement of hardness and high-temperature wear resistance of laser-clad CoAlTiWTa RHEA coating on inconel 718 superalloy by addition of TiC
|
|
Xiaolian Liu, Ke Zhu, Ning Guo
|
59 |
38 |
18196–18214 |
2024 |
5.83 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Corrosion resistance tailoring of a paramagnetic Ti–6Al–4V through a static magnetic field exposure in solid state
|
|
Priyanka Agrawal, Sanya Gupta, Rajiv S. Mishra
|
59 |
38 |
18215–18226 |
2024 |
6.77 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Metallic ions integrated in tannic acid (TA) as a metal–organic-like complex coating on biodegradable magnesium for enhanced corrosion control and biocompatibility
|
|
Jiacheng Wang, Zhenglong Dou, Nan Huang
|
59 |
38 |
18227–18245 |
2024 |
0.0 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Atomic-scale investigation on diffusion mechanism of immiscible Mo/Cu system under different temperatures and electric field
|
|
Yunqi Lu, Xiaolin Guo, Jiaqian Tong
|
59 |
38 |
18246–18262 |
2024 |
6.84 |
|
平均評価: 0.0 / 5
(0 件のレビュー)
|
|
Tunable zinc corrosion rate by laser surface modification for implants with controllable degradation direction
|
|
Peng Chen, Yazhou Hu, Chunyong Liang
|
59 |
38 |
18263–18277 |
2024 |
6.84 |
|
平均評価: 0.0 / 5