Defining the Role of Hot Band Annealing in High-Permeability Grain-Oriented (GO) Electrical Steel
|
|
Sushil K. Giri, Saurabh Kundu, Indradev Samajdar
|
53 |
5 |
1873–1888 |
2022 |
14.42 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
Correction to: An Investigation into Sinterability Improvements of 316L Binder Jet Printed Parts
|
|
Rasim Batmaz, Ali Zardoshtian, Etienne Martin
|
53 |
5 |
1919–1919 |
2022 |
14.31 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
On the Competitive Substitutional Partitioning During Nano-pearlitic Transformation in Multicomponent Steels
|
|
Snehashish Tripathy, P. S. Manoranjan Jena, Sandip Ghosh Chowdhury
|
53 |
5 |
1806–1820 |
2022 |
13.75 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
On the Optimization of the Microstructural and Mechanical Properties of Model Ni-Based Superalloys Through the Alloying Effects of Refractory Mo and W Elements
|
|
Rasim Eriş, M. Vedat Akdeniz, Amdulla O. Mekhrabov
|
53 |
5 |
1859–1872 |
2022 |
13.45 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
Microstructural Evolution in Additively Manufactured Fe-Cr-Ni Maraging Stainless Steel
|
|
Ayda Shahriari, Mehdi Sanjari, Mohsen Mohammadi
|
53 |
5 |
1771–1792 |
2022 |
12.75 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
Effect of Zr or Ga Addition and Annealing on Microstructural Evolution, Deformation and Fracture Behaviour of Nb-19Si-5Mo-20Ti Based Hypereutectic Alloy
|
|
Kasturi Sala, Rahul Mitra
|
53 |
5 |
1717–1737 |
2022 |
12.71 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
Molar Volume and Surface Tension of Liquid Bi–Cu Alloys
|
|
Janusz Pstruś, Przemyslaw Fima
|
53 |
5 |
1659–1673 |
2022 |
12.36 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
High-Temperature Cycle Deformation and Fracture Behavior of Advanced Austenitic Heat-Resistant Steel Sanicro25 Alloy for A-USC Power Plants
|
|
Dechao Lyu, Tieshan Cao, Jie Zhao
|
53 |
5 |
1738–1748 |
2022 |
11.82 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
Cold Drawing of Commercially Pure Titanium and Its Effect on Microstructure and Texture Evolution
|
|
B. Bishoyi, R. Vinjamuri, S. K. Sahoo
|
53 |
5 |
1845–1858 |
2022 |
11.6 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|
|
High-Throughput Experiment and Numerical Simulation to Study Solidification Cracking in 2195 Aluminum Alloy Welds
|
|
M. Agilan, K. Satyamshreshta, G. Phanikumar
|
53 |
5 |
1906–1918 |
2022 |
11.38 |
|
Average Rating: 0.0 / 5
(0 Reviews)
|